Skip to content
Delta Structures
EstimateFree estimate
KNOWLEDGE HUB · 112 FREE FIELD GUIDES

Know before you build.

Plain-language guides from our engineering desk. No jargon without a translation and no scare tactics, just the checks and rules of thumb professionals use on site, so you can talk to any contractor, including us, as an informed client.

You have read 0 of 112 guides
DID YOU KNOW15 OF 36

Differential settlement, not settlement itself, is what cracks buildings – the problem is uneven movement.

FROM THE GUIDE Structural crack vs shrinkage crack

Showing 12 of 112 guidesAll 112 guides

No guides match “”.Try a broader word such as damp, cement or RERA, or ask Delta below.
DID YOU KNOW · 1 OF 210

Rust expands 4-6 times the steel it grows from - that expansion is what pops the concrete off old Kolkata buildings.

These guides describe standard Indian construction practice and field checks aligned with IS codes, such as IS 456 for concrete, IS 383 for aggregates and IS 1893 for seismic zoning. They are general education. Every building is different, so treat anything structural as a reason for an on-site professional assessment, not a do-it-yourself diagnosis.

ASK DELTA · ENGLISH · বাংলা · हिंदी

Still have a question?

Ask in English, Bengali or Hindi. Answers come from these guides, with the source named.

Ready to plan your own build?

Five taps give you a cost range, a season plan and your area’s rules. Or send us your plot for a free preliminary estimate, usually within 48 hours.*

*Indicative, not guaranteed. Timing varies with the complexity of your query.

Search or ask Delta
CIVIL WORKS· 13 MIN READ
এই গাইডটি এখনও শুধু ইংরেজিতে।

5 on-site brick quality checks

Red clay bricks of the kind used on building sites across India
Photo: Ramesh NG, CC BY-SA 2.0, via Wikimedia Commons
THE SHORT ANSWER

Good bricks ring, survive a drop, don't drink like a sponge, and match each other. You can test all of this at delivery in ten minutes, before a single brick goes into your wall.

IN PLAIN WORDS

Checking bricks at delivery is like checking eggs at the shop — trivial before you buy, impossible to undo after they're in the cake.

A brick wall is only as good as the bricks that go into it. Badly fired bricks crumble, drink water, carry salts that bloom through the plaster, and make the mortar joints thick and weak. Good bricks are hard, regular, ring when struck and take up only a modest amount of water. The difference is easy to see at the truck and very expensive to put right once the bricks are in the wall and plastered over.

This guide explains what makes a good brick, what the Indian standard asks of common burnt clay bricks, the kinds of bricks you will be offered in and around Kolkata, the checks you can make in ten minutes at delivery and the ones that need a day, when to send bricks to a laboratory, how bricks should be stored and laid, and what to do with a load that fails. It is meant to help you or your site supervisor check what arrives; for load-bearing walls, the brick strength is part of the design and your engineer sets it.

What makes a good brick

A clay brick is moulded from clay and silt, dried, and fired in a kiln. Firing turns the clay into a hard ceramic. Fire it too little and the centre stays weak and soft, absorbs water like a sponge and breaks down in a wet wall. Fire it too much and it melts and warps into the dark, glassy, misshapen bricks known in Bengal as jhama, hard but irregular. A good brick sits between the two: fired right through, hard, and regular in size and shape.

Four properties decide how a brick behaves in a wall. Strength decides how much load it can carry. Water absorption decides how much water it draws from the mortar and from rain and damp, which affects the bond and the wall's resistance to damp. Soluble salts decide whether white deposits will bloom on the wall and push off the plaster. And regularity of size and shape decides how thin and even the mortar joints can be, which affects the wall's strength, its look and how much mortar it uses.

What the Indian standard asks

IS 1077 is the Indian specification for common burnt clay building bricks. It sorts bricks into classes by their average compressive strength, from class 3.5 (3.5 N/mm²) up to class 35, and sets limits for each class on water absorption and efflorescence, the white salt deposit. It also sets standard sizes and how far a batch may vary from them. The methods for testing strength, absorption, efflorescence and warping are in the four parts of IS 3495, and how many bricks to pick for testing is in IS 5454.

The traditional size on most Indian sites is 230 × 110 × 70 mm, the non-modular size the standard keeps alongside the modular 190 × 90 × 90 mm. Many kilns in Bengal still make bricks closer to the old local size of about 10 × 5 × 3 inches, and sizes vary from kiln to kiln. What matters most on site is that the bricks in one load match each other.

Compressive strengthWHAT IS 1077 ASKSThe class is the average strength in N/mm², from 3.5 to 35; no single brick far below itWHY IT MATTERSLoad-bearing walls need the class the design calls for
Water absorption (24 hours in cold water)WHAT IS 1077 ASKSNot more than 20% of the dry weight up to class 12.5; not more than 15% for higher classesWHY IT MATTERSThirsty bricks weaken the mortar bond and let damp through
EfflorescenceWHAT IS 1077 ASKSNot more than moderate up to class 12.5; not more than slight for higher classesWHY IT MATTERSSalts in the brick bloom through plaster and paint
Size (20 bricks in a row)WHAT IS 1077 ASKS230 × 110 × 70 mm bricks: 4,600 ± 80 mm long, 2,200 ± 40 mm wide, 1,400 ± 40 mm high; 190 × 90 × 90 mm: 3,800 ± 80, 1,800 ± 40, 1,800 ± 40 mmWHY IT MATTERSRegular bricks give thin, even joints
AppearanceWHAT IS 1077 ASKSHand or machine moulded, free from cracks, flaws and nodules of free lime; sharp, square edgesWHY IT MATTERSLime nodules swell when wet and burst the brick

The bricks you will be offered around Kolkata

Most clay bricks used in and around Kolkata come from kilns in the districts around the city, many of them along the rivers, where the clay and silt of the delta make good brick earth. They are usually sold by local grade rather than by IS class. First-class bricks are the well-fired, regular, deep red ones that ring when struck; second-class bricks are slightly irregular in shape or colour but still well fired; lower grades include under-fired, pale bricks that should not go into walls. Jhama bricks, over-fired and misshapen, are not used for walls but are broken up for brick-bat soling under floors and for the brick aggregate known as khoa.

Ask for the grade in writing, and if the bricks are going into load-bearing walls, ask whether the kiln can give a test certificate for strength and absorption. Many cannot, which is one reason to test a sample yourself.

You may also be offered alternatives. Fly ash bricks, pressed from fly ash with lime or cement, are made to IS 12894; they are regular in size, light grey, and their quality depends heavily on the maker. Aerated autoclaved concrete (AAC) blocks, made to IS 2185 Part 3, are much lighter and larger and are laid with a thin adhesive; our guide to AAC blocks and brick compares the two. Each has its own checks, and the clay brick checks below do not all apply to them.

Workers loading fired bricks onto a tractor trailer at a brick field in India
Photo: McKay Savage, CC BY 2.0, via Wikimedia Commons

The ten-minute delivery check

These checks need nothing more than a tape, a hard floor and your hands, and they should be done before the truck leaves. Pick bricks at random from different parts of the load, not from the top or from a stack the driver offers you.

  1. 1Look at the whole load: one colour and one shape, no mix of two batches, few broken bricks, no pale or yellowish bricks among the red ones.
  2. 2Ring test: strike two bricks together, or tap one with a steel rod. A well-fired brick gives a clear, ringing sound; a dull thud means under-fired or cracked bricks.
  3. 3Scratch test: try to scratch the face with a fingernail. A good brick does not mark; a soft, under-fired one does.
  4. 4Drop test: drop a brick flat from about one metre onto hard ground. It may chip at a corner, but it should not break into pieces.
  5. 5Break one: split a brick in two and look at the inside. It should be uniform in colour and dense right through, with no black or soft core, no large holes and no white lumps of lime.
  6. 6Size check: lay 20 bricks end to end on a level floor and measure the total length, then lay them side by side for width and stacked for height, and compare with the standard's limits for their size. Then check a few bricks for straight edges and flat faces.

The overnight checks

Two more checks take a day but tell you a great deal. They follow the idea of the IS 3495 laboratory tests in a simple form you can do on site; they are a screening, not a certified test.

  1. 1Water absorption: take three dry bricks, weigh each on a kitchen or shop scale, soak them in clean water for 24 hours, wipe the surface water off and weigh them again. The weight gained divided by the dry weight is the absorption. Well-fired common bricks should stay at or under about 20%.
  2. 2Efflorescence: stand a few bricks on end in a shallow tray with about 25 mm of clean water and leave them in a warm, airy place until the water has been drawn up and dried out. Look at the surfaces: none or only a thin trace of white deposit is good; white covering a large part of the brick, or powdering and flaking, means salts that will show on your walls.
  3. 3Record the results with photographs and the date, and keep the tested bricks aside. If a load fails, the record is what you show the supplier.

When to send bricks to a laboratory

For load-bearing walls, compound walls of any height, and any building where the engineer has specified a brick class, the strength should be confirmed by a laboratory test, not just by the ring and the drop. The standard method is in IS 3495 Part 1: the bricks are soaked, their frogs filled with mortar, and they are crushed in a testing machine; the class is the average of a set. The same laboratory can test water absorption and efflorescence by the standard methods.

How many bricks to send, and how to pick them from a large lot, is set out in IS 5454. In practice your engineer or the laboratory will tell you how many to bring and how to mark them. Test early, from the first loads, and again if the supplier or kiln changes.

Storing and using bricks on site

Good bricks can still be spoiled on site. Stack them on firm, level ground or planks, not on bare soil where they can draw up water and salts, in neat stacks that do not topple, near where they will be used to cut down handling. Unload them by hand or onto a soft surface; tipping them from a truck breaks corners and causes hidden cracks.

Clay bricks are soaked in water before they are laid, as IS 2212 on brickwork asks, so that they do not draw the water out of the mortar before it can set and bond. They should be wet through but not dripping when laid. Fly ash bricks and AAC blocks follow their makers' instructions, which are different. Joints should be filled solid, generally around 10 mm thick, and the finished brickwork kept moist for about a week so that the mortar cures.

  • Stack on planks or firm ground, never on wet soil or next to a salty drain.
  • Unload by hand; do not tip bricks from the truck.
  • Soak clay bricks before laying, and let surface water drain off.
  • Keep bricks from different loads apart until each has been checked.
  • Keep the finished brickwork moist for about a week.
Bricks stacked beside a foundation trench in a village in Ratnagiri district, Maharashtra
Photo: urbzoo, CC BY 2.0, via Wikimedia Commons

Problems that start with a bad load

Many of the problems homeowners see years later trace back to the bricks. White, powdery patches that keep returning on new plaster are often salts from the bricks themselves, especially when the bricks were stored on wet ground or the walls were wetted heavily. Damp that soaks through outer walls in the monsoon is worse in walls of thirsty, under-fired bricks. Small pits and craters on plaster, appearing a few months after the work, can be lime nodules in the bricks swelling as they take up moisture.

Irregular bricks make thick, uneven joints, which use more mortar, make the wall weaker and lead to more plaster to hide the unevenness, and with it more cracking. And bricks that are too weak for a load-bearing wall can crush under concentrated loads, such as under a beam or at the ends of a lintel. All of these are cheaper to prevent with a few minutes of checking than to cure after the wall is built.

What to do with a load that fails

Reject at the truck, not at the wall. Once bricks have been unloaded and mixed with good ones, it is hard to return them and harder to prove which were bad. If a load fails the delivery checks, do not accept it, note why on the delivery slip, and photograph the bricks and the slip.

  • A dull sound across many bricks in the ring test, or bricks that scratch easily.
  • Pale, yellowish or uneven colours, or a mix of two different batches.
  • Black or soft cores, white lime lumps or large holes when a brick is broken.
  • Many broken, cracked or warped bricks in the load.
  • A 20-brick row well outside the standard's limits.
  • Heavy white deposits on bricks already in the stack.
  • No grade, kiln name or invoice with the load.

The 10-minute delivery test

  1. 1Ring test: strike two bricks together — a clear metallic ring means well-fired; a dull thud means under-burnt.
  2. 2Drop test: drop one flat from about chest height onto hard ground — it may chip but shouldn't shatter.
  3. 3Absorption: weigh a brick, soak 24 hours, weigh again — it shouldn't gain more than about 20% of its weight (per IS 1077 for common clay bricks). A brick that drinks heavily weakens mortar bond and invites damp.
  4. 4Shape & size: edges straight, faces flat, sizes consistent across the lot — wildly varying bricks mean thick, wasteful mortar joints.
  5. 5Colour & salts: uniform deep red/brown; white powdery patches signal salts that will later bloom through your plaster.

Questions people ask

What is a first-class brick?

A local trade grade, not an IS class. It usually means a well-fired, deep red brick of regular size and shape with sharp edges, that rings when struck and does not absorb much water. It is a good sign, but for load-bearing walls ask for the IS strength class or test a sample.

Are darker bricks always better?

Not always. A deep, even red usually means good firing, but very dark, glassy, twisted bricks are over-fired jhama, which are too irregular for walls. Pale bricks are usually under-fired. Look for an even colour across the load and check with the ring, scratch and break tests.

Is a little white powder on new bricks a problem?

A light trace that brushes off is common. A heavy white coating, or bricks that powder or flake, mean soluble salts that will come through your plaster. Do the efflorescence check on a few bricks, and keep the bricks off wet ground.

Why do bricks need to be soaked before laying?

A dry clay brick draws water out of the mortar so fast that the mortar cannot set properly and bond to it. Soaking first, as IS 2212 asks, gives a stronger, better-bonded wall. Fly ash bricks and AAC blocks have their own rules from their makers.

Should we use fly ash bricks or AAC blocks instead?

Both have their place: fly ash bricks are regular and suit many walls, and AAC blocks are much lighter, which helps on upper floors and on weak soils. Their quality varies by maker and they need their own checks. Our guide to AAC blocks and brick compares them.

How many bricks does your wall need?

Our Brick, Block and Mortar tool in the Lab works it out for your walls, with openings and wastage, and includes the 20-brick check for the delivery.

RED FLAGS ON SITE
  • Dull thud on the ring test across many bricks
  • White salt patches on a large share of the lot
  • Two visibly different batches mixed in one delivery
PRO TIP

Reject at the truck, not at the wall. Our supply arm does exactly these checks before material is accepted on any Delta site.

WORK IT OUT · FREE CALCULATORBrick & Mortar CalculatorWall size → bricks, cement, sandOpen the calculator →
QUIZ · THREE QUESTIONS

Did it stick?

QUESTION 1 OF 3 What does a clear ring when two bricks are struck tell you?
Ask our engineers on WhatsApp
Sources · checked 15 Nov 2026
  1. IS 1077:1992 Common Burnt Clay Building Bricks, SpecificationChecked 15 Nov 2026
  2. IS 3495 (Parts 1 to 4):1992 Methods of Tests of Burnt Clay Building BricksChecked 15 Nov 2026
  3. IS 5454:1978 Methods for Sampling of Clay Building BricksChecked 15 Nov 2026
  4. IS 2212:1991 Code of Practice for BrickworkChecked 15 Nov 2026
  5. IS 12894:2002 Pulverized Fuel Ash Lime Bricks, SpecificationChecked 15 Nov 2026

Checked against these sources on the dates shown, pending our team’s sign-off. Rules change, so we check them again for your plot before anything is filed.