Skip to content
Delta Structures
EstimateFree estimate
KNOWLEDGE HUB · 112 FREE FIELD GUIDES

Know before you build.

Plain-language guides from our engineering desk. No jargon without a translation and no scare tactics, just the checks and rules of thumb professionals use on site, so you can talk to any contractor, including us, as an informed client.

You have read 0 of 112 guides
DID YOU KNOW15 OF 36

Differential settlement, not settlement itself, is what cracks buildings – the problem is uneven movement.

FROM THE GUIDE Structural crack vs shrinkage crack

Showing 12 of 112 guidesAll 112 guides

No guides match “”.Try a broader word such as damp, cement or RERA, or ask Delta below.
DID YOU KNOW · 1 OF 210

Rust expands 4-6 times the steel it grows from - that expansion is what pops the concrete off old Kolkata buildings.

These guides describe standard Indian construction practice and field checks aligned with IS codes, such as IS 456 for concrete, IS 383 for aggregates and IS 1893 for seismic zoning. They are general education. Every building is different, so treat anything structural as a reason for an on-site professional assessment, not a do-it-yourself diagnosis.

ASK DELTA · ENGLISH · বাংলা · हिंदी

Still have a question?

Ask in English, Bengali or Hindi. Answers come from these guides, with the source named.

Ready to plan your own build?

Five taps give you a cost range, a season plan and your area’s rules. Or send us your plot for a free preliminary estimate, usually within 48 hours.*

*Indicative, not guaranteed. Timing varies with the complexity of your query.

Search or ask Delta
MATERIALS· 12 MIN READ
এই গাইডটি এখনও শুধু ইংরেজিতে।

The 10-minute silt test for sand

A heap of building sand delivered to a site
Photo: Jonathan Hutchins, CC BY-SA 2.0, via Wikimedia Commons
THE SHORT ANSWER

Silt and clay coat sand grains and weaken the bond in concrete and mortar. Field rule aligned with IS 383: settled silt should be roughly under 8% of the sand column in a simple jar test. Also: never sea sand for structure — its salt corrodes reinforcement from day one.

IN PLAIN WORDS

Silt in sand is like dust on tape — the tape is fine, it just won't stick. Cement paste can't grip a dirty grain.

Sand makes up a large part of every mortar, plaster and concrete mix, and it is the material most often accepted without a second look. Yet dirty sand is one of the commonest reasons for weak plaster, crumbling joints, cracked screeds and concrete that misses its strength. The fine silt and clay in it coat the grains so that cement cannot grip them, take up extra water, and shrink as they dry. A simple jar of water, left on a windowsill for an hour, shows most of what you need to know.

This guide explains what silt and clay do to mortar and concrete, what the Indian standard asks of sand, the jar test and other checks you can make on site, how to read the result, the other problems to look for (salt, organic matter, poor grading and bulking), the kinds of sand offered around Kolkata, and what to do with a load that fails. It is meant for owners and site supervisors; the mixes themselves are set by your engineer.

What silt and clay do

In a good mix, every grain of sand is coated with cement paste, and the paste bonds the grains to each other and to the stone. Silt and clay are particles far finer than sand. When they are present in quantity, they stick to the sand grains as a dusty film, so the paste bonds to the film instead of to the grain. The bond is weaker, and it gets weaker still when the clay swells with water and shrinks as it dries.

Fine particles also have a huge surface area, so they soak up water. A mason working with silty sand adds more water to make the mix workable, which raises the water to cement ratio and lowers the strength. Silty mortar and plaster shrink more as they dry and crack more. In concrete, excess fines can also reduce durability, because the extra water leaves more pores for water and air to travel through to the steel.

  • Weaker bond between the cement paste and the grains.
  • More water needed for the same workability, so lower strength.
  • More drying shrinkage and cracking in plaster, screeds and joints.
  • Patchy, powdery plaster surfaces that dust and do not hold paint well.
  • More porous concrete, less protection for the steel.

What the standard asks

IS 383, the Indian standard for coarse and fine aggregates for concrete, limits the amount of very fine material in sand, measured as the share by weight that passes a 75 micron sieve, and the amount of clay lumps and other harmful material. Its limits are much tighter for natural sand, where the fines are usually silt and clay, than for manufactured sand, where the fines are mostly crushed rock dust, which is less harmful. The test methods are in IS 2386. IS 383 also sorts fine aggregates into grading zones by the sizes of their grains, which the engineer uses to choose sand for concrete.

For masonry mortar and plaster, IS 2116 sets out what the sand should be like, with its own grading. In both cases the laboratory tests are by weight on dried samples, which is not what a jar test on site measures. The jar test is a quick screen: if it shows a lot of silt, the sand should be rejected or sent for a laboratory test.

The jar test, step by step

The jar test, sometimes called the field settling test, needs a clear straight-sided glass or plastic jar, water, a little salt and an hour or so. Take the sample from several places in the heap, not just the surface, and mix it.

  1. 1Fill a clean, clear, straight-sided jar with the sand sample to about a quarter or a third of its height.
  2. 2Add clean water until the jar is about three quarters full, and a teaspoon of salt, which helps the fine particles settle into a clear layer.
  3. 3Close the jar and shake it hard for a minute, so that every grain is separated and washed.
  4. 4Stand it on a level surface and leave it alone for at least an hour, preferably three.
  5. 5Look at the side of the jar: the sand settles first at the bottom, and the silt settles on top of it as a distinct, finer, usually darker or lighter layer.
  6. 6Measure the height of the silt layer and of the sand below it with a ruler.
  7. 7Divide the silt height by the sand height and multiply by 100 to get the silt percentage by volume.
  8. 8Note the water too: water that stays muddy for hours means a lot of clay.

Other quick checks

A few more checks take a minute each and catch problems the jar test does not. Do them on the same sample.

  • Rub test: rub a handful of damp sand between your palms. Clean sand leaves little behind; sand that stains your hands brown or grey and leaves a sticky film carries clay or silt.
  • Squeeze test: squeeze a handful of damp sand and open your hand. Clean sand falls apart; clayey sand holds its shape like dough.
  • Look at the grains: they should be hard, clean and mostly of mixed sizes, without lumps of clay, bits of wood, leaves, shells or rubbish.
  • Smell and colour: a musty smell or black specks suggest organic matter, which slows cement setting.
  • Taste or touch for salt: a salty taste or a white crust as the heap dries are warnings of sea or estuary sand, or sand stored on salty ground.

Salt and sea sand

Sand from the sea or from tidal river mouths carries salt, mostly chlorides. Chlorides in concrete attack the steel inside it, starting corrosion that cracks and spalls the concrete years later. IS 456 limits the total chloride content of concrete for this reason. Salt in plaster and mortar also draws moisture from the air and blooms on the wall as a white crust. Sea sand should never be used in reinforced concrete, and should not be used in mortar or plaster unless it has been washed and tested.

Shells, very rounded and uniform grains, and a salty taste are the signs to look for. If a supplier cannot tell you where the sand came from, or the price is far below others for the same kind, ask more questions.

Grading, fineness and bulking

Clean sand can still be the wrong sand. Good concrete sand has a range of grain sizes, so that smaller grains fill the gaps between larger ones and less cement paste is needed. Very fine, uniform sand needs more water and more cement for the same mix, and gives weaker, more shrinkage-prone concrete. That is why fine sand, often sold for filling or plaster, should not be used for concrete unless the engineer approves it after a grading test.

Damp sand also takes up more volume than dry sand, because the film of water on each grain pushes the grains apart. This bulking can make damp sand take up a fifth to a third more volume than the same sand dry, depending on its fineness and moisture. On sites where sand is measured by the box or the head pan rather than weighed, bulked sand means less sand in the mix than intended. Engineers allow for this by measuring the bulking or by using dry or saturated sand; it is one reason weigh batching is better.

The sand you will be offered around Kolkata

Sand for building in and around Kolkata comes mainly from riverbeds in the surrounding districts and from manufactured sand plants that crush rock. Suppliers usually sell it by local names for coarse and fine sand rather than by IS zone. Coarse river sand is used for concrete and masonry; finer sands are sold for plaster and for filling. The quality varies from load to load, even from one supplier, because the source and the depth it was dug from change. Every new source deserves its own test.

Manufactured sand, made by crushing and grading rock, is a legitimate alternative when it is well graded, washed or air-classified to control its dust, and made from sound rock. It should be judged by the same tests as river sand, not by preference either way. Our guide to M-sand and river sand compares the two in detail, and our guide to aggregate checks covers the stone.

A loader filling a lorry with dredged sand near Mumbai
Photo: Sumaira Abdulali, CC BY-SA 3.0, via Wikimedia Commons

Reading the result

The jar test gives you a number and a picture, and the two together tell you what to do. Keep the jar and a photograph of it with the date and the supplier's name, so you can compare loads and show the supplier the result if it fails.

Silt layer under about 3%WHAT IT USUALLY MEANSClean sandWHAT TO DOAccept, if the other checks are clean
About 3 to 8%WHAT IT USUALLY MEANSSome silt; usually acceptable for most workWHAT TO DOAccept for mortar and plaster; for concrete, follow the engineer's limit or test it
Over about 8%WHAT IT USUALLY MEANSSilty or clayey sandWHAT TO DOReject, or have it washed and tested before use
Water still muddy after hoursWHAT IT USUALLY MEANSA lot of clayWHAT TO DOReject for structural work

Washing and rejecting

Silty sand can be washed on site by spreading it on a sloping, clean surface or in a trough and running water through it until the water runs clear, then letting it drain. It works, but it is slow, uses a lot of water, and needs space and labour. For concrete, it is usually better to reject a silty load than to wash it. If you do wash sand, test it again afterwards.

Reject at the truck, not at the mixer. Once a silty load has been tipped onto a clean heap, the two are mixed and both are spoiled. Do the rub and squeeze checks as the truck arrives, run the jar test on the first load from every new source, and note any rejection on the delivery slip with a photograph.

  • Store sand on a clean, hard, drained base, away from soil, drains and salty ground.
  • Keep coarse and fine sand in separate heaps, clearly marked.
  • Cover heaps in heavy rain so the fines do not wash in from around them.
  • Test the first load from every new source, and again if a load looks different.
  • Reject silty or salty loads, and record why.

The jar test, step by step

  1. 1Fill a clear glass jar about half with the sand sample.
  2. 2Add water until nearly full, plus a pinch of salt (helps silt settle distinctly).
  3. 3Shake hard for a minute, then leave undisturbed for 1–3 hours.
  4. 4Silt settles as a distinct fine layer on top of the sand. Measure both: silt layer ÷ sand height × 100.
  5. 5Under ~8%: acceptable. Above: reject or require washing.

Two more quick checks

  • Rub test: rub damp sand between palms — heavy staining means excessive clay/silt.
  • M-sand (manufactured sand) is a legitimate river-sand alternative when properly graded — judge it by the same silt/cleanliness tests, not by prejudice either way.

Questions people ask

How much silt is too much?

As a site rule of thumb, a settled silt layer of more than about 8 percent of the sand height in a jar test is too much for most work, and less is better for concrete. The engineer may set a tighter limit, and the standard's laboratory test is by weight, which reads lower than the jar.

Why add salt to the jar?

A little salt helps the very fine particles clump and settle into a clear layer on top of the sand, so the silt is easier to see and measure.

Can silty sand be used for plaster?

A little silt is tolerated in plaster, but silty sand makes plaster shrink, crack and dust more. For plaster that has to last, use clean sand of the right fineness, or wash it first.

Is M-sand safe for concrete?

Yes, when it is made from sound rock, well graded and controlled for dust, and when it passes the same tests as river sand. Our guide to M-sand and river sand explains what to check.

Why does the same sand seem to change volume?

Damp sand bulks: the water film on each grain pushes them apart, so a box of damp sand holds less sand than a box of dry sand. That is why weighing is better than measuring by the box.

How much sand does your work need?

Our calculators work out sand for plaster, mortar and concrete, and our Brick, Block and Mortar tool in the Lab does the same for your walls.

RED FLAGS ON SITE
  • Sand that stains hands heavily
  • A whitish crust or salty taste-of-air around the heap (possible sea sand)
  • Visible mud lumps in the load
PRO TIP

One jar, water, and an hour — the cheapest quality test in construction. We run it on every sand source before approval.

WORK IT OUT · FREE CALCULATORPlaster Material CalculatorWall area → cement & sandOpen the calculator →
QUIZ · THREE QUESTIONS

Did it stick?

QUESTION 1 OF 3 In the jar test, about how much settled silt is acceptable?
Ask our engineers on WhatsApp
Sources · checked 15 Nov 2026
  1. IS 383:2016 Coarse and Fine Aggregate for Concrete, SpecificationChecked 15 Nov 2026
  2. IS 2386 Methods of Test for Aggregates for ConcreteChecked 15 Nov 2026
  3. IS 2116:1980 Sand for Masonry Mortars, SpecificationChecked 15 Nov 2026
  4. IS 456:2000 Plain and Reinforced Concrete, Code of Practice (chlorides in concrete)Checked 15 Nov 2026

Checked against these sources on the dates shown, pending our team’s sign-off. Rules change, so we check them again for your plot before anything is filed.